Treatability Performance of Kempas, Eucalyptus and Pine Sleepers with Coal-Tar Creosote

Show simple item record

dc.contributor.author Karunathilake, E.M.B.M.
dc.contributor.author Amarasekera, H.S.
dc.contributor.author Dewendra, M.C.
dc.date.accessioned 2017-04-03T04:32:44Z
dc.date.available 2017-04-03T04:32:44Z
dc.date.issued 2015
dc.identifier.citation Karunathilake, E.M.B.M., Amarasekera, H.S., & Dewendra, M.C. (2015). Treatability Performance of Kempas, Eucalyptus and Pine Sleepers with Coal-Tar Creosote. Proceedings of the 20th International Forestry and Environment Symposium, University of Sri Jayewardenepura, Nugegoda, 20, 49. en_US, si_LK
dc.identifier.uri http://dr.lib.sjp.ac.lk/handle/123456789/4709
dc.description.abstract Treating wood with coal tar creosote increases its service life by preventing biological deterioration. For the present study, creosote, major oil borne preservative was used to treat railway sleepers. In Sri Lanka, State Timber Corporation import Kempas railway sleepers from Malaysia and re-export to Singapore after treating them with coal tar creosote in creosote: furnace oil ratios of 90:10 or 80:20. Eucalyptus sleepers are also treated with coal tar creosote in creosote: furnace oil ratio of 50: 50 according to the BS 144 Standards. Furnace oil acts as a carrier of creosote and increase the penetration and retention of preservatives in wood. The effect of creosote:furnace oil ratios of 90:10, 80:20, 70:30 and 50:50 on penetration and retention of Kempas, Eucalyptus and Pinus sleepers were measured with and without incising using 5×5×45 cm sample poles. Retention is the quantity of creosote remaining in the poles after the treatment which should not be less than 115 kg/m3 according to the BS144 standards. Average retention of creosote furnace oil mixture of 50:50 in incised Kempas poles was found to be 157.43 kg/m3. Pine had the retention value of 320.85 kg/m3 even without incising while Eucalyptus showed the retention value of 48.11 kg/m3 without incising which is below the standard value. The moisture content was below 25%. Penetration refers to how deeply the preservative enters the wood which should not be less than 2.2 cm, according to the BSEN 351-1:1995 standard. Incised Kempas showed 2.067 cm penetration while Eucalyptus and Pine showed 0.679 cm and 2.200 cm without incising. Pine (soft wood species) showed the higher penetration and retention values compared with Eucalyptus. Kempas (hardwood species) had higher penetration and retention values than Eucalyptus after incision. en_US, si_LK
dc.language.iso en en_US, si_LK
dc.publisher University of Sri Jayewardenepura, Nugegoda en_US, si_LK
dc.subject Creosote en_US, si_LK
dc.subject Retention en_US, si_LK
dc.subject Penetration en_US, si_LK
dc.subject Pressure treatment en_US, si_LK
dc.subject Kempas en_US, si_LK
dc.subject Eucalyptus en_US, si_LK
dc.subject Pine en_US, si_LK
dc.title Treatability Performance of Kempas, Eucalyptus and Pine Sleepers with Coal-Tar Creosote en_US, si_LK